M.P. Mikhailova Handbook Series on Semiconductor Parameters, vol.1, M. Levinshtein, S. Rumyantsev and M. Shur, ed., World Scientific, London, 1996, pp. 147-168.
Adachi, S., J. Appl. Phys. 66, 12 (1989) 6030-6040.
Aspnes, D. E. and A. A. Studna, Phys. Rev.B27, 2 (1983) 985-1009.
Barm, I., 0. Knacke, and 0. Kubaschewski, Thermochemical Properties of Inorganic Substances, Springer, Berlin, 1977.
Blaut-Blachev, A. N., L. A. Balagurov, V. V. Karataev, and E. M. OmePyanovskii, Sov. Phys. Semicond.9, 4 (1975) 515-516.
Brennan, K. and K. Hess, Solid State Electron.27, 4 (1984) 347-357.
Burenkov, Yu. A., S. Yu. Davydov, and S. P. Nikanorov, Sov. Phys. Solid State17, 7(1975) 1446-1447.
Caries, R.,N. Saint-Cricq, J. B. Renucci, M. A. Renucci, and A. Zwick, Phys. Rev.B22, 10 (1980) 4804-4815.
Dixon, J. R., Proc. 5th Int. Conf. on Physics of Semiconductors, Prague, 1961, p. 366.
Dixon, J. R. and J. M. Ellis, Phys. Rev. 123, 5 (1961) 1560-1567.
Domanskaya, L. I., M. I. Iglitsyn, E. V. Soloveva, and I. M. Tsidilkovskii, Sov. Phys. Semicond.3 (1970) 1548.
Edwards, A. L. and H. G. Drickamer, Phys. Rev.122, 4 (1960) 1149-1157.
Fang, Z. M., K. Y. Ma, D. H. Jaw, R. M. Cohen, and G. B. Stringfellow, J. Appl. Phys.67, 11 (1990) 7034-7039.
Garyagdyev, G., 0. V. Emel'yanenko, N. V. Zotova, T. S. Lagunova, D. N. Nasledov, and A. V. Pentsov, Sov. Phys. Semicond.8 (1974) 335.
GeFmont, B. L., Z. N. Sokolova, and I. N. Yassievich, Sov. Phys. Semicond.16, 4 (1982) 592-600.
Guseva, M. I., N. V. Zotova, A. V. Koval, and D. N. Nasledov, Sov. Phys. Semicond.8 10 (1975) 1323.
Guseva, M. I., N. V. Zotova, A. V. Koval, and D. N. Nasledov, Sov. Phys. Semicond.8, 1 (1974) 34-36.
Jain, S. L., J. M. McGregor, and D. J. Roulston, J. Appl. Phys.68, 7 (1990) 3747-3749.
Kamakura, K., T. Akashi, and M. Tsuzuki, J. Phys. Soc. Jpn.38, 5 (1975) 1383-1388.
Karataev, V. V., M. G. Mil'vidsky, N. S. Rytova, and V. I. Fistui, Sov. Phys. Semicond 11, 9 (1977) 1009-1011.
Kesamanly, F. P., T. S. Lagunova, D. N. Nasledov, L. A. Nikolaeva, and M. N. Pivovarov, Fiz. i Tekhn. Polupr.2, 1 (1968) 56-63 (in Russian).
Kesamanly, F. P., Yu. MaTtsev, D. N. Nasledov, L. A. Nikolaeva, M. N. Pivovarov, V. A. Skripkin, and Yu. I. Uvanov, Fiz. Tekhn. Polupr.3, 8 (1969) 1182-1187 (in Russian). Krotkus, A. and Z. Dobrovolskis, Electrical Conductivity of Narrow-Gap Semiconductors, Vilnus, Mokslas, 1988.
Kuchar, F., G. Bauer, and H. HiUbrand, Phys. Status Solidi (A)17, 2 (1973) 491-496.
Lorimor, 0. G. and W. G. Spitzer, J. Appl. Phys.36, 6 (1965) 1841-1847.
Mikhailova, M. P., A. A. Rogachev, and I. N. Yassievich, Sov. Phys. Semicond.10, 8 (1976) 866-871.
Okhotin, A. S., A. S. Pushkarskii, and V. V. Gorbachev, Thermophysteal Properties of Semiconductors "Atom" Publ. House, Moscow, 1972, (in Russian).