InN. Calculated steady-state drift velocity as function of electric
field at different doping concentrations Nd . T = 300 K. Nd (cm-3): 1 - 1017 cm-3; 2 - 1018cm-3; 3 - 1018cm-3 O'Leary et al. (1998) |
![]() |
InN. Calculated steady-state drift velocity as a function of electric
field at different temperatures T. Doping concentration Nd = 1017 cm-3. T (K): 1 - 150 K; 2 - 300 K; 3 -500 K O'Leary et al. (1998) |
![]() |
InN, Wurtzite. Calculated average electron energy as a function of
electric field. Continuous lines - applied electric field along Γ - M directions. Dashed lines - applied electric field along Γ - A directions. Bellotti et al. (1999). |