Electron αi and hole βi ionization
coefficients in Ga0.47In0.53As versus 1/F. Osaka et al. (1985) |
![]() |
Electron αi and hole βi ionization
Ga0.8In0.2As - GaAs strained layer superlattice versus 1/F. Bhattacharya et al. (1986) |
![]() |
Avalanche breakdown voltages for Ga0.47In0.53As (curve 1) and InP (curve 2) p+ -n abrupt junctions
versus carrier concentration. Arnold et al. (1984) |